slaked for 24 hours, and gauged with water coloured with ochre, so as to give a creamy tone when the plaster dries out: or, 3 of selenitic cement to 2 of silver sand, both sifted as above—this may be used for out-door work.

Individual taste and experience must decide as to the thickness of the final coat, but if laid between ⅛ and 112 inch, and the lines cut with slanting edges, a side light gives emphasis to the finished result, making the outlines tell alternately as they take the light or cast a shadow. Plasterers' small tools of various kinds and knife-blades fixed in tool handles will be found suited to the simple craft of cutting and clearing off the final surface coat; but as to this a craftsman finds his own tools by experience, and indeed by the same acquired perception must be interpreted all the foregoing directions, and specially that ambiguous

166